I also tried a two-stage slip resist naked raku again; I dipped burnished bisqueware with waxed bottoms into slip, let it dry until it began to crack, and then dipped it in clear glaze before firing. I first tried one- and two-step slip resist naked raku out in April 2024, with mostly very low-contrast results. This time, I had higher contrast results, but also let some the slip dry too long before doing the clear glaze dip, as some of it actually touched the clay surface in a number of areas on the larger oval bowl and a couple on the smaller bowl (both below). Though it wasn’t intended, if it’s widespread like it is on the oval bowl, I actually am visually into the result (much like I am into crazing/crawling, which are also considered glaze defects).
Here’s the little dish, which has the highest contrast I’ve produced in slip resist naked raku:
And here’s the larger oval bowl: